Korundon mawon
Deskripsyon
Korundum mawon, ke yo rele tou Emery, se te fè nan boksit, materyèl kabòn ak pousyè tè apre rediksyon fonn nan gwo founo dife a ak mawon oksid aliminyòm, konpozisyon chimik prensipal la se AL2O3, kontni li se 95. 00 pousan {{ 4}}.00 pousan. Ak dapre engredyan yo nan alumina, li divize an diferan nivo. Abrazif Brown Fused Alumina ak bon boksit kòm matyè premyè, ak anthracite, fichye fè nan arc la pa 2000 degre pi wo a fusion tanperati ki wo, fanm k'ap pile ak fòme, fè separasyon mayetik, ekran nan yon varyete granularite, teksti dans li yo, segondè dite, patikil. boul fòmasyon, apwopriye pou fabrikasyon seramik, résine segondè ak zouti abrazif ak fanm k'ap pile, polisaj, sablaj, Distribisyon presizyon, elatriye, kapab tou itilize yo fabrike materyèl refractory.
Brown fusion alumina tou gen gwo chaj ralantisman tanperati ak estabilite volim tanperati ki wo lè manifakti pwodwi yo. Sepandan, enpurte a nan BFA detèmine lavi sa a ki depo nan pwodwi a nan pwosesis la nan itilize. Paske enpurte yo pa te konplètman retire nan pwosesis la Distribisyon, alumina mawon fusion tou gen faz segondè cristalline. An jeneral, pwosesis la Distribisyon ak tan nan korundon mawon detèmine pèfòmans nan ak bon jan kalite nan pwodwi a.
Karakteristik
Korundum Brown konpayi nou an gen karakteristik pite segondè, bon kristalizasyon, likidite fò, koyefisyan ekspansyon lineyè ki ba, rezistans korozyon. Pwodwi a gen karakteristik pa gen okenn inisyasyon, pa gen okenn pulverizasyon ak pa gen okenn fann nan pwosesis aplikasyon an.
Pwodwi Deskripsyon
|
Aplikasyon |
Spesifikasyon |
Konpozisyon chimik prensipal pousan |
Pousan sibstans mayetik |
||||
|
Al2O3 |
Fe2O3 |
SiO2 |
TiO2 |
||||
|
Abrazif |
F |
4#—80# |
Pi gran pase oswa egal a 95 |
Mwens pase oswa egal a 0.3 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 3.0 |
Mwens pase oswa egal a 0.05 |
|
90#—150# |
Pi gran pase oswa egal a 94 |
Mwens pase oswa egal a 0.03 |
|||||
|
180#—240# |
Pi gran pase oswa egal a 93 |
Mwens pase oswa egal a 0.3 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 3.5 |
Mwens pase oswa egal a 0.02 |
||
|
P |
8#—80# |
Pi gran pase oswa egal a 95.0 |
Mwens pase oswa egal a 0.2 |
Mwens pase oswa egal a 1.2 |
Mwens pase oswa egal a 3.0 |
Mwens pase oswa egal a 0.05 |
|
|
100#—150# |
Pi gran pase oswa egal a 94.0 |
Mwens pase oswa egal a 0.03 |
|||||
|
180#—220# |
Pi gran pase oswa egal a 93.0 |
Mwens pase oswa egal a 0.3 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 3.5 |
Mwens pase oswa egal a 0.02 |
||
|
W |
1#-63# |
Pi gran pase oswa egal a 92.5 |
Mwens pase oswa egal a 0.5 |
Mwens pase oswa egal a 1.8 |
Mwens pase oswa egal a 4.0 |
— |
|
|
REFRACTORY |
Duansha |
0-1mm 1-3mm 3-5mm 5-8mm 8-12mm |
Pi gran pase oswa egal a 95 |
Mwens pase oswa egal a 0.3 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 3.0 |
— |
|
25-0mm 10-0mm 50-0mm 30-0mm |
Pi gran pase oswa egal a 95 |
Mwens pase oswa egal a 0.3 |
Mwens pase oswa egal a 1.5 |
— |
|||
|
poud |
180#-0 200#-0 320#-0 |
Pi gran pase oswa egal a 93.5 |
Mwens pase oswa egal a 0.5 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 3.5 |
— |
|
Aplikasyon
Abrazif: BFA se youn nan abrazif enpòtan, yo ka itilize pou fanm k'ap pile metal, seramik, vè ak lòt materyèl dite segondè.
Tretman andigman: Li ka itilize kòm yon materyèl tretman sifas, itilize yo retire korozyon nan sifas la metal, kouch oksid.
Materyèl REFRACTORY: Brown Fused Alumina gen bon rezistans dife, yo ka itilize nan envantè de brik REFRACTORY, kouch REFRACTORY, elatriye.
Materyèl elektwonik: Corundum mawon gen pwopriyete izolasyon ekselan, yo ka itilize pou fabrike materyèl izolasyon elektrik, sikui entegre, elatriye.
Tretman dlo: Li ka itilize pou tretman dlo, itilize pou retire enpurte ak polyan nan dlo, amelyore kalite dlo.
Lòt aplikasyon: Brown Fused Alumina kapab tou itilize nan envantè de Meservey atifisyèl, seramik, fib vè ak lòt materyèl.
Anbalaj ak anbake
Anbalaj selon sekirite lanmè-ekspòtasyon anbalaj estanda
Dispatch: chaje materyèl anbalaj fini nan faktori pa veso Pòt an Pòt
Pa 25kg sak papye kraft plis lanmè fumigate palettes an bwa

Baj popilè: mawon corundum, Lachin mawon corundum manifaktirè, Swèd, faktori